Executive SummaryA wheel core decides four things more specific than load capacity: moment of inertia, structural deformation, corrosion resistance and machining consistency.
At equal dimensions, an aluminium core weighs roughly one third of a carbon steel core, and its moment of inertia falls in the same proportion. This follows from density, not from a test result.
Aluminium is not universally better. High impact loads, tight cost targets and volume production each give carbon steel or cast iron a defensible case.
Bond strength depends more on the surface preparation of the core than on the tread compound itself.
The correct order of selection is load, then speed and dynamic demand, then environment, then process route, then cost. Cost comes last.
Before the detail, here is the conclusion, so you can map it against your own application and decide whether the rest of this article applies to you.
An aluminium core suits medium to light loads where dynamic response matters and precision requirements are higher. Its value is not lightness in itself but the reduction in inertia that lightness brings: faster acceleration, more repeatable stopping, lower energy draw. AGV drive wheels are the clearest beneficiaries of this logic.
A carbon steel core suits heavy loads, cost sensitive projects and moderate to good precision requirements. It has ample strength and machines easily, but it is heavy and needs corrosion protection. Fitted to equipment that demands fast dynamic response, it works against you.
A cast iron core suits heavy loads, low running speeds and applications with visible vibration or impact. Its advantages are stiffness and damping, and casting lends itself to volume production at a low unit cost. The price is tooling, which makes small batches uneconomic.
These three materials are not related as good to bad. They are related as matched to mismatched. The cost of choosing wrongly is rarely a wheel that fails outright. More often it is equipment that will not position accurately, energy consumption that runs higher than it should, or a maintenance schedule that keeps coming back.
Most enquiries about wheel cores ask one question: will it hold up. That matters, but the influence of the core on the machine runs well beyond load capacity. Breaking it into four areas is the only way to see the real cost of a material decision.
This is the factor most often left out, and the one with the largest effect on AGV behaviour.
A rotating wheel has to overcome its own moment of inertia. For a wheel close to a solid cylinder, this can be estimated as J = ½mr². Inertia scales with mass, and with the square of the radius. At equal dimensions, halving the mass halves the inertia.
The formula carries two practical implications. First, reducing core weight lowers inertia linearly, so the return on a lighter material is predictable. Second, increasing wheel diameter raises inertia quadratically, which is why a larger wheel cannot be chosen on load capacity alone. A larger wheel rolls more easily but carries considerably more inertia, and for equipment with a tight cycle time the trade is often a losing one.
The densities involved are approximately 2.7 g/cm³ for aluminium, 7.85 for carbon steel and 7.2 for cast iron. At equal dimensions and comparable structural proportions, an aluminium core is about one third the weight of a carbon steel core, and its moment of inertia is about one third as well. This is the physical reason aluminium became the default in AGV design. It is not a question of a premium material. The properties happen to match what the application needs.
The benefits of lower inertia appear in three places. Drive torque demand during acceleration falls, so the same battery delivers more range. Braking distance shortens, so positioning converges more easily. And in duty cycles with frequent starts and stops, the load on motor and gearbox is reduced.
One honest caveat belongs here. The inertia of the wheels is only part of the inertia of the whole vehicle, and the share depends on total mass. For an AGV weighing several hundred kilograms, the difference between four aluminium wheels and four steel wheels may amount to only a few percent of total inertia. The energy saving should therefore not be overstated. In duty cycles with high start-stop frequency and tight cycle times, however, the difference is real and measurable in throughput.
Aluminium has lower yield strength than carbon steel, which is well known. In a wheel core application, two distinct failure modes need to be separated: deformation caused by insufficient overall strength, and fatigue caused by local stress concentration.
Overall strength is governed by the thinnest section. If the web of the core is designed sensibly and wall thickness is adequate, an aluminium core performs well under medium loads. The problem usually appears at the bearing seat, where a thin ring of material carries highly concentrated compressive stress. Insufficient strength in aluminium shows up as gradual enlargement of the bearing seat, which ends in a loose bearing and a wheel that runs out of true.
Carbon steel and cast iron hold the advantage at this location. Cast iron has moderate tensile strength, but its compressive strength and stiffness are good, so the bearing seat resists deformation. This is a major reason heavy load applications lean toward cast iron and steel.
This is where carbon steel is weakest. Without surface treatment, a carbon steel core rusts quickly in a damp environment. The rust layer occupies space in the bearing fit and also interferes with bonding to the polyurethane.
The usual answers are zinc plating, black oxide or painting, and each has limits. Zinc plating protects well but adds thickness, which affects fit tolerance. Black oxide is inexpensive but offers limited protection. Paint cannot be used on bearing seats or on bonding surfaces at all.
Aluminium has useful corrosion resistance without additional treatment, and anodising improves it further while producing a uniform appearance. Anodised layers are typically in the range of ten or so microns, so the effect on fit dimensions can be controlled.
Cast iron sits between the two, but its surface is porous. Once corrosion starts, it follows the graphite structure inward. In damp conditions, surface treatment for a cast iron core is not optional.
Aluminium and carbon steel are machined, so dimensional accuracy and part-to-part consistency are straightforward to control. This suits small and medium batches and custom designs.
Cast iron is cast in one operation, which lowers unit cost at volume, but casting tolerances are coarser than machining tolerances and critical fits usually need a secondary machining pass. Casting also requires a mould, and tooling cost and lead time are the main obstacle at low volume.
This point causes frequent misunderstanding in practice. A customer asks whether a cast iron core can be made in a quantity of two. The answer is yes, but two wheels would have to carry the cost of a full set of tooling, which makes the unit price far higher than either an aluminium or a steel machined core. The sensible recommendation is to start with a machined design at low volume and convert to casting only once the quantity is established.
HANKE confirms the process route against the customer drawing before quoting: aluminium and steel cores are machined, cast iron cores are tooled and cast. The two routes are priced separately and clearly, so a low volume requirement is never compared against a volume production unit price.
The four areas above condense into a single table. The entries read as relative, not absolute values; the actual selection always depends on the specific structural design.
Parameter | Aluminium | Carbon steel | Cast iron |
Density (g/cm³, approx.) | 2.7 | 7.85 | 7.2 |
Weight at equal size | About 1/3 | Reference | About 0.92 |
Yield strength | Below carbon steel | High | Moderate tensile, high compressive |
Bearing seat stability | Moderate | Good | Good |
Damping | Moderate | Moderate | Good |
Corrosion resistance (bare) | Reasonable | Poor, treatment required | Moderate, porous surface |
Surface treatment | Anodising | Zinc plating / black oxide / paint | Primer / paint / plating |
Forming route | Machining | Machining | Casting plus critical-face machining |
Tooling cost | None | None | Mould required |
Small batch economics | Good | Good | Poor |
Volume economics | Moderate | Moderate | Good |
Typical fit | Medium to light load, high dynamics | Heavy load, cost sensitive | Heavy load, low speed, vibration |
There is a shortcut to reading this table. Look at the tooling cost and small batch economics rows first, and half the unsuitable options eliminate themselves. Many projects spend a long time comparing materials when the batch size already decided, at requirement stage, whether casting was ever available.
In AGV design, aluminium is close to a default. That default has conditions attached: the equipment must be sensitive to dynamic response, the load must sit in the medium range, and the batch must be neither very small nor enormous. Outside those conditions, aluminium is not automatically the right answer.
Transport equipment with frequent starts and stops is the natural home for aluminium. Every acceleration and every stop has to overcome wheel inertia, so the higher the start-stop frequency, the more visible the cost of inertia becomes. AGVs, AMRs and shuttle vehicles all fall into this category.
Equipment with tight positioning requirements also benefits. A light wheel produces a smaller inertial impulse during braking, which makes it easier for the control system to settle at the target position. The effect is clearest where a vehicle has to dock repeatedly against the same rack.
Applications involving manual handling or frequent wheel changes gain as well. Halving the weight of a wheel makes a noticeable difference to maintenance, particularly where technicians lift wheels out of position rather than rolling them along a bench.
Impact loads call for caution. Forklifts, drop impacts and vehicles crossing rails or thresholds at speed all put transient loads through the bearing seat. Under those conditions an aluminium core deforms more readily, and carbon steel or cast iron is the safer specification.
Heavy loads are also a poor fit. Once per-wheel load enters the tonne range, the strength margin of aluminium becomes tight. Achieving comparable strength requires thicker walls, which erodes the weight advantage until steel becomes the more efficient choice.
Extremely cost-driven projects are the third case. Aluminium costs more in both material and machining than carbon steel. Where the equipment is highly cost sensitive and dynamic performance is not critical, an aluminium core is over-specified.
For bonding aluminium to polyurethane, surface preparation decides the outcome. Aluminium readily forms a dense oxide layer, and that layer obstructs the formation of chemical bonds. An aluminium core therefore needs dedicated surface treatment before coating, with grit blasting to increase roughness and effective bond area.
At HANKE, aluminium cores are grit blasted and then primed, and the primer thickness is measured to confirm uniform coverage before the casting stage begins. The order cannot be reversed. A process that casts first and repairs the interface afterwards cannot correct a defect that has already formed.
The timing of anodising is a second consideration. Anodising must be completed before coating, and the anodised layer must not extend over the bonding surface, or bond strength drops significantly. Errors of process sequence like this surface most often during first-article trials, when the finishing steps are still being established.
Carbon steel is the least selective of the three materials. It has sufficient strength, machines easily and is inexpensive, so it works in almost any application. The price is weight and the need for corrosion protection.
A generous strength margin is the core advantage. At equal dimensions, a carbon steel core carries significantly more load than an aluminium one, giving adequate safety margin in heavy duty applications without forcing a complicated structural design.
Machinability matters in practice. Turning, milling, drilling and tapping are all straightforward, so custom designs move through production quickly and tolerances are easy to hold. For prototype stages and small to medium orders, that responsiveness is a real commercial advantage rather than a technical footnote.
Cost is the third factor. Both material and machining cost less than aluminium, and the gap widens at volume.
Weight cannot be changed, only offset through structural design: lightening holes or reduced wall thickness in non-load-bearing regions. Both raise process complexity and introduce stress concentration, so a strength check is required. Material should not be removed on the basis of intuition.
Corrosion protection is mandatory, and the method should follow the service environment. In dry indoor conditions, black oxide or a simple paint coat is adequate. In damp or washdown environments, zinc plating or a switch to stainless steel is more appropriate. Surface treatment changes fit dimensions, so bearing seats and bonding surfaces need allowance on the drawing.
Bonding surface preparation is equally important. Rust and oil on a carbon steel surface destroy adhesion directly, so degreasing, descaling and grit blasting are all required before coating. None of the three can be skipped.
HANKE sequences carbon steel cores as follows: surface treatment and corrosion protection first, bonding surface preparation second, casting last. This order ensures the protective layer never contaminates the bond interface, and it avoids having to redo surface treatment after the polyurethane has been cast.
Cast iron is often treated as the low-end option among wheel core materials. That is a misreading. Cast iron has physical advantages nothing else substitutes for; its applicability is simply narrower than aluminium or steel.
Stiffness and damping. The graphite structure in cast iron absorbs vibration, which is valuable where the duty cycle includes visible impact or shaking: scrubber dryers, sweepers, forklifts and transport equipment running on uneven floors. In those conditions a cast iron core usually runs more steadily than a steel one.
Compressive strength is high. The bearing seat carries compressive stress, and cast iron performs well in that direction, resisting the gradual enlargement that eventually loosens a bearing.
Casting suits volume. A single forming operation reduces machining hours, so unit cost falls as quantity rises. This is the economic core of the case for cast iron.
Cast iron requires tooling. Mould cost and tooling lead time are the practical threshold for small batch projects, and they are usually the first thing to clarify in a quotation discussion.
In commercial conversations this needs explaining clearly. Two wheels can certainly be made, but two wheels have to absorb the cost of a full mould, which pushes the unit price far above an aluminium alternative. The useful recommendation is therefore not that casting is possible, but that the quantity is better served by a machined design first, with a conversion to casting once the volume justifies it.
HANKE tooling and casts cast iron cores to customer drawings and completes the coating in the same process. Before tooling starts, three things are confirmed: how the core is loaded, the bearing fit dimensions, and whether machining allowance should be left on the casting. Settling these early avoids repeated mould corrections later.
Cast iron has a porous surface and often contains free graphite, both of which weaken chemical bonding at the interface. Pre-treatment requirements are therefore stricter than for aluminium or steel. Grit blasting must remove the surface graphite and rust completely to expose fresh metal, and the primer should be applied immediately afterwards to prevent re-oxidation.
Reworked parts are where this most often goes wrong. If a cast iron core recovered from a used wheel has already corroded, a light sanding followed by re-coating will not deliver reliable bond strength. Whether rework is worthwhile depends on corrosion depth, not on how smooth the surface looks.
Beyond the three mainstream materials, one category of application needs separate treatment: highly corrosive environments and locations with strict cleanliness requirements.
Stainless steel cores offer the highest corrosion resistance and suit food processing, pharmaceutical production, chemical handling and equipment that is washed down frequently. The cost is higher material and machining expense, with weight falling between aluminium and steel.
Bonding stainless steel is the difficult part. The passive layer obstructs chemical bond formation just as the aluminium oxide layer does, and pre-treatment requirements are stricter than for aluminium. Where a project calls for a stainless core, the bonding process should be confirmed as a separate item before first articles are made. Assuming it behaves like aluminium is a common and expensive mistake.
Application | Recommended core | Key constraint |
Food processing, frequent washdown | Stainless steel | Corrosion resistance critical, bonding pre-treatment confirmed separately |
Pharmaceutical, cleanroom | Stainless steel or anodised aluminium | Dense surface, no shedding, cleanable |
Chemical handling | Stainless steel | Compatibility to be confirmed against the specific medium |
Outdoor, damp, salt spray | Anodised aluminium or zinc plated carbon steel | Coating thickness affects fit dimensions |
Cold storage | Aluminium or carbon steel, low-temperature toughness checked | Material toughness at low temperature must be confirmed |
A second special requirement is electrical insulation or static dissipation. This is normally solved through the tread compound rather than the core material, but the conductive path between core and bearing has to be considered at the same time. A dissipative tread on an otherwise insulated assembly achieves nothing.
The preceding sections condense into a sequence you can work through. The order matters more than the individual steps.
Step | What to confirm | Why it sits here |
1 | Load per wheel, presence of impact load | Sets the strength requirement and eliminates materials that cannot carry it |
2 | Running speed, start-stop frequency, positioning tolerance | Establishes how much inertia matters, and therefore how much aluminium buys you |
3 | Service environment: humidity, washdown, chemical exposure | Sets the corrosion protection route, and whether stainless steel enters the picture |
4 | Batch size, whether the design is custom | Decides machining versus casting, and whether tooling can be amortised |
5 | Budget and lead time | Final arbitration among the options already screened by steps one to four |
The order of steps one and two deserves emphasis. Many enquiries begin by asking whether to use aluminium or steel, which treats the conclusion as the starting point. The correct sequence establishes load and dynamic requirements first, lets those two conditions screen the field, and only then discusses material preference.
Step four is the one most often skipped and most often responsible for rework. Batch size determines the process route, the process route determines the cost structure, and the cost structure feeds back into material choice. Leaving batch size until the end means every comparison done earlier may have to be redone.
The most frequent errors of judgement are listed below, each with a short correction. Every row is expanded in the paragraphs that follow.
Common assumption | What is wrong with it | Better approach |
Aluminium is always better than steel | Its advantage is concentrated in inertia, which only matters where dynamics are critical | Start with load and start-stop frequency |
A heavier core is a stronger core | Weight and strength are different properties, and structural design often dominates | Look at section design and wall thickness |
Cast iron is cheaper, so prefer it | The unit cost advantage depends on volume | Calculate total cost including tooling amortisation |
Surface treatment is cosmetic | It affects fit dimensions and bond strength | Specify the process at drawing stage |
Core and tread can be chosen separately | The two are joined into one part through the bond interface | Confirm both together, in one decision |
The advantage of aluminium is concentrated in inertia, and inertia only carries value where dynamics are critical. For slow, heavy, continuously running equipment, aluminium delivers limited benefit while charging a premium for strength margin that the application does not need.
Weight and strength are not the same property. Cast iron is heavier than aluminium but has lower tensile strength than carbon steel. Structural design influences load capacity at least as much as material does, and an under-thickness steel core is not necessarily more durable than a well-designed aluminium one.
The unit cost advantage of cast iron rests on volume. At low quantities, tooling amortisation can push the total cost of a cast iron core well above a machined aluminium or steel alternative. Calculate the total, not the material price per kilogram.
Zinc plating and anodising exist primarily to prevent corrosion; appearance is secondary. Both also change fit dimensions and affect bond strength, which means the process has to be decided at drawing stage rather than added after machining is complete.
The core governs load capacity and precision, the tread governs traction and wear, and the bond interface joins them into a single part. A well-chosen core bonded through an inadequate process delivers no better service life than a poorly chosen one. The two decisions belong together.
Once the core material is settled, three parameters still need confirming alongside the tread.
The first is the relationship between tread hardness and core stiffness. A soft tread on an insufficiently stiff core produces uneven contact pressure and accelerates localised wear. A hard tread on a core with adequate stiffness gives a more uniform contact condition. The relationship becomes most visible under heavy load.
The second is the structural design of the bond interface. Surface roughness, the presence or absence of grooves or knurling, and whether edges are chamfered all affect interface strength. HANKE uses a chemical bonding interface, in which pre-treatment allows the polyurethane to form a chemical bond with the metal rather than relying on mechanical interlocking alone. In normal service the difference shows up as strength margin. Under repeated impact or frequent washdown, it shows up as reliability.
Interface factor | What to confirm | Consequence if mismatched |
Tread hardness vs core stiffness | Soft tread needs a core with adequate stiffness | Uneven contact pressure, faster localised wear |
Bond interface geometry | Surface roughness, grooves or knurling, edge chamfers | Insufficient interface strength, becomes the failure origin |
Timing of surface treatment | Anodising or plating completed before coating | Treatment layer covers the bond surface, strength drops sharply |
Dimensional inspection | Full-dimensional check of the core on a CMM | Concentricity out of tolerance after batch assembly |
The third is inspection. HANKE confirms core dimensional accuracy through full-dimensional inspection on a coordinate measuring machine, and hardness is confirmed at multiple points to establish distribution uniformity. Both matter in volume supply, because core consistency directly determines how the assembled batch performs.
At HANKE, every batch of cores is checked for dimensions and surface treatment condition before entering the casting stage, and finished wheels are inspected for hardness and appearance before dispatch. Wear performance is tested to DIN 53516, which provides a basis for comparing compounds against one another. That figure describes the difference between materials; it does not convert into a service life in a particular workshop.
HANKE matches tread compounds to application through two systems: HANKE Eamflex 93A high-wear-resistance compound for demanding abrasion, and HANKE Saxflex 75A floor-protection compound where grip and floor condition matter more than tread life. Which of the two suits a given core and duty cycle is a question for the application data, not a default.
Q1: Does an AGV wheel have to use an aluminium core?
No. The advantage of aluminium is low inertia, which only delivers a clear benefit where start-stop frequency is high and positioning tolerance is tight. For slow, heavy, continuously running equipment, a steel or cast iron core is often the better match, with more strength margin and a lower cost.
Q2: How much lighter is an aluminium core than a steel one?
At equal dimensions and comparable structural proportions, aluminium has roughly one third the density of carbon steel, so an aluminium core weighs about one third as much. Real parts deviate from that ratio because of lightening holes, bearing seats and other structural differences, so the actual figure has to be calculated from the drawing.
Q3: How much does core weight affect AGV battery life?
It depends on the share of wheel weight in total vehicle weight. Wheel inertia is only part of total inertia, so for a vehicle weighing several hundred kilograms the effect of a weight difference across four wheels is limited. It becomes more visible in duty cycles with frequent starts and stops, and less visible in continuous running at steady speed.
Q4: Why does a cast iron core need tooling, and can it be made in small quantity?
Cast iron parts are formed by casting, which requires a mould. Small quantities are possible, but the tooling cost spread across a few parts makes the unit price high. The usual recommendation is to start with a machined design and convert to casting once the quantity is established.
Q5: What should be done if a carbon steel core has rusted?
It depends on where the rust is and how deep it goes. If corrosion is confined to non-critical surfaces, it can be removed and the surface treatment renewed. If corrosion has reached the bearing fit or the bonding surface, both dimensional accuracy and bond strength are compromised, and replacement is usually more economical than rework.
Q6: Can a stainless steel core be supplied, and what are the limits?
Yes. Stainless steel offers the highest corrosion resistance and suits food, pharmaceutical and frequent washdown applications. The limits are cost and bonding. The passive layer on stainless steel interferes with chemical bonding, so pre-treatment requirements are stricter than for aluminium and the process should be confirmed before trial parts are produced.
Q7: How should core material and tread hardness be matched?
The principle is to match stiffness with hardness. A soft tread needs a core stiff enough to support it, otherwise uneven contact pressure accelerates localised wear. A hard tread on an adequately stiff core gives a more uniform contact condition. The specific combination has to be confirmed against load distribution and duty cycle.
Q8: How can the machining quality of a wheel core supplier be assessed?
Three things are worth asking for: a dimensional inspection report for the core, a clear description of the bonding surface preparation, and a willingness to confirm the process route at trial stage rather than quoting immediately. Suppliers who can answer all three usually have genuine control over the process. HANKE provides all three as a standard part of a quotation.
Wheel core selection goes wrong so often because it looks like a materials question when it is really a matching question. The physical properties of aluminium, carbon steel and cast iron are fixed. Whether they perform well depends on whether they line up with what the equipment actually needs.
The right question is therefore not which material is better, but what the load, cycle time, environment and batch size of this particular machine are. Answer those four and the material follows almost automatically. What remains is process detail.
HANKE works with all three core materials and completes the polyurethane coating in the same process. Core dimensions are confirmed on a coordinate measuring machine, the bond interface is a chemical bonding system rather than mechanical interlocking, and tread compounds are drawn from HANKE Eamflex 93A and HANKE Saxflex 75A systems depending on duty cycle. The specific combination of material and structure still has to be confirmed against the customer drawing and the actual operating conditions.